Free of salt high-pressure deliming of animal hides.

阅读:8
作者:Prokein Michael, Chrobot Adrian, Renner Manfred, Weidner Eckhard
The wastewater pollution of tanneries is of high concern. The investigation of technologies to minimize the consumption of chemicals in the leather production process can reduce the environmental burden. We focus on the reduction of ammonium salts in the leather production process. Salt-free deliming of animal hides with compressed carbon dioxide as deliming agent is performed for the first time in a technical scale 20-L drum. As a result, CO(2)-deliming at 30 bar and 30 °C is two times faster than conventional deliming. In addition, the deliming efficiency is slightly improved. The initial calcium (Ca) content of the hides of 8 g/kg reaches the lowest value of 2 g/kg after a process time of 3 h. However, a process time of 60 min is sufficient to reach an elimination of 50 wt% of the initial lime. The resulting Ca-content of 4 g/kg after 60 min CO(2)-deliming at 30 bar is comparable with the Ca-content of conventional delimed hide. We clarify that the ampholytic character of the collagen itself enables a buffering of the pH-value at pH-7. The stable pH-value supports the selection of specific bating enzymes that decompose non-collagen proteins. No buffering salts contaminate the wastewater. The high-pressure CO(2)-deliming process has high potential to reduce wastewater emissions, save costs for chemicals, and process time in industrial beamhouse applications.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。