Effect of pore size in bone regeneration using polydopamine-laced hydroxyapatite collagen calcium silicate scaffolds fabricated by 3D mould printing technology

利用3D模具打印技术制备聚多巴胺掺杂羟基磷灰石胶原硅酸钙支架,研究孔径大小对骨再生的影响

阅读:1

Abstract

OBJECTIVE: The pore size of the scaffold is a critical factor in repairing large bone defect. Here, we investigated the potential of bone regeneration using novel nanocomposite polydopamine-laced hydroxyapatite collagen calcium silicate (HCCS-PDA) scaffolds with two different pore sizes, 250 and 500 μm. SAMPLES/SETTING: A total of 12 male Sprague-Dawley rats were implanted with HCCS-PDA scaffold with pore size of either 250 or 500 μm into surgically created critical-sized defect (CSD). METHODS: HCCS-PDA scaffolds were fabricated using mould printing technique. The effect of pore size on mechanical strength of the scaffolds was assessed by compression testing. After seeding with rat mesenchymal stem cells (rMSCs), the scaffolds were implanted, and new bone formation was evaluated using microCT and histomorphometric analysis after 8 weeks. RESULTS: MicroCT and histology analysis demonstrated restricted peripheral new bone formation in either dural or periosteal side and limited new bone formation in the 250 μm pore scaffold. Conversely, the 500-μm pore scaffold showed more penetration of new bone into the scaffold and greater bone regeneration in the rat CSD. CONCLUSION: Based on our results, which demonstrated improved new bone formation in 500 μm pores scaffold, we can conclude that effective scaffold pore size that induces osteointegration and bone regeneration is around 500 μm for HCCS-PDA nanocomposite scaffold.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。