As most plastic materials disintegrate without being properly reused after they are discarded, this present study developed a novel thermoplastic elastomer (TPE) using recycled high-density polyethylene (rHDPE) and natural rubber (NR) with kenaf fibre as a sustainable filler. Apart from being used as filler, this present study aimed to examine the use of kenaf fibre as a natural anti-degradant as well. The results indicated that the tensile strength of the samples was found to have significantly decreased after 6 months of natural weathering and had decreased by a further 30% after 12 months due to the chain scission of the polymeric backbones and the degradation of the kenaf fibre. However, the composites that contained kenaf fibre significantly retained their properties post-natural weathering. In terms of tensile strength and elongation at the break, the addition of only 10 phr of kenaf increased the retention properties by 25% and 5%, respectively. This is noteworthy as kenaf fibre also contains a certain amount of natural anti-degradants. Therefore, as the kenaf fibre improves the weather resistance of composites, plastic manufacturers could use it as either a filler or a natural anti-degradant.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。