The inevitable gap between in vitro and in vivo degradation rate of biomaterials has been a challenging factor in the optimal designing of scaffold's degradation to be balanced with new tissue formation. To enable non-/minimum-invasive tracking of in vivo scaffold degradation, chemical modifications have been applied to label polymers with fluorescent dyes. However, the previous approaches may have limited expandability due to complicated synthesis processes. Here, we introduce a simple and efficient method to fluorescence labeling of polymeric scaffolds via blending with near-infrared (NIR) quantum dots (QDs), semiconductor nanocrystals with superior optical properties. QDs-labeled, 3D-printed PCL scaffolds showed promising efficiency and reliability in quantitative measurement of degradation using a custom-built fiber-optic imaging modality. Furthermore, QDs-PCL scaffolds showed neither cytotoxicity nor secondary labeling of adjacent cells. QDs-PCL scaffolds also supported the engineering of fibrous, cartilaginous, and osteogenic tissues from mesenchymal stem/progenitor cells (MSCs). In addition, QDs-PCL enabled a distinction between newly forming tissue and the remaining mass of scaffolds through multi-channel imaging. Thus, our findings suggest a simple and efficient QDs-labeling of PCL scaffolds and minimally invasive imaging modality that shows significant potential to enable in vivo tracking of scaffold degradation as well as new tissue formation.
Quantum dots-labeled polymeric scaffolds for in vivo tracking of degradation and tissue formation.
量子点标记的聚合物支架用于体内跟踪降解和组织形成
阅读:5
作者:Sim Kun Hee, Mir Mohammad, Jelke Sophia, Tarafder Solaiman, Kim Jinho, Lee Chang H
| 期刊: | Bioactive Materials | 影响因子: | 20.300 |
| 时间: | 2022 | 起止号: | 2022 Mar 17; 16:285-292 |
| doi: | 10.1016/j.bioactmat.2022.03.003 | 研究方向: | 其它 |
特别声明
1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。
2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。
3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。
4、投稿及合作请联系:info@biocloudy.com。