The influence of the etching method on the occurrence of defect levels in InAs/InAsSb type-II superlattice (T2SLs) and MCT photodiode is presented. For both analyzed detectors, the etching process was performed by two methods: wet chemical etching and dry etching using an ion beam (RIE-reactive ion etching). The deep-level transient spectroscopy (DLTS) method was used to determine the defect levels occurring in the analyzed structures. The obtained results indicate that the choice of etching method affects the occurrence of additional defect levels in the MCT material, but it has no significance for InAs/InAsSb T2SLs.
The Influence of Etching Method on the Occurrence of Defect Levels in III-V and II-VI Materials.
阅读:9
作者:Majkowycz Kinga, Murawski Krzysztof, Kopytko MaÅgorzata, Nowakowski-Szkudlarek Krzesimir, Witkowska-Baran Marta, Martyniuk Piotr
| 期刊: | Nanomaterials | 影响因子: | 4.300 |
| 时间: | 2024 | 起止号: | 2024 Oct 9; 14(19):1612 |
| doi: | 10.3390/nano14191612 | ||
特别声明
1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。
2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。
3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。
4、投稿及合作请联系:info@biocloudy.com。