Sand-casting is a well established primary process for manufacturing various parts of A356 alloy. However, the quality of the casting is adversely affected by the change in the magnitude of the control variables. For instance, a larger magnitude of pouring velocity induces a drop effect and a lower velocity increases the likelihood of cold-shut and mis-run types of defects. Similarly, a high pouring temperature causes the formation of hot tears, whereas a low temperature is a source of premature solidification. Likewise, a higher moisture content yields microcracks (due to gas shrinkages) in the casting and a lower moisture content results in the poor strength of the mold. Therefore, the appropriate selection of control variables is essential to ensure quality manufactured products. The empirical relations could provide valuable guidance in this regard. Additionally, although the casting process was optimized for A356 alloy, it was mostly done for a single response. Therefore, this paper aimed to formulate empirical relations for the contradictory responses, i.e., hardness, ultimate tensile strength and surface roughness, using the response surface methodology. The experimental results were comprehensively analyzed using statistical and scanning electron microscopic analyses. Optimized parameters were proposed and validated to achieve castings with high hardness (84.5 HB) and strength (153.5 MPa) with minimum roughness (5.8 µm).
Modelling the Mechanical Attributes (Roughness, Strength, and Hardness) of Al-alloy A356 during Sand Casting.
阅读:10
作者:Ishfaq Kashif, Ali Muhammad Asad, Ahmad Naveed, Zahoor Sadaf, Al-Ahmari Abdulrahman M, Hafeez Faisal
| 期刊: | Materials | 影响因子: | 3.200 |
| 时间: | 2020 | 起止号: | 2020 Jan 28; 13(3):598 |
| doi: | 10.3390/ma13030598 | ||
特别声明
1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。
2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。
3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。
4、投稿及合作请联系:info@biocloudy.com。