This study evaluated the effectiveness of chemical-based adhesive techniques on promoting immediate and aged bond strength between zirconia and luting cement. A total of 128 discs of zirconia were divided into 4 groups (n = 32) according to the adhesive treatment: tribochemical silica-coating followed by silane (Silane Primer, Kerr) and bonding (Optibond FL, Kerr), Signum Zirconia Bond (Hereaus), Z-Prime Plus (Bisco), and All-Bond Universal (Bisco). Composite cylinders were cemented on the zirconia sample with Duo-Link Universal (Bisco). Eight specimens per group were subjected to 10,000 thermocycles and subsequently bond strength was tested with shear-bond strength test. ANOVA test showed that artificial aging significantly affected the bond strength to zirconia. Bonferroni test highlighted a significant influence of adhesive treatment (Signum) on bond strength after thermocycling. It was concluded that 10-MDP-based bonding systems showed no improvement in initial bond strength compared with tribochemical treatment. All chemical bonding techniques tested in this study were influenced by thermocycling.
Do Chemical-Based Bonding Techniques Affect the Bond Strength Stability to Cubic Zirconia?
阅读:6
作者:Comba Allegra, Baldi Andrea, Tempesta Riccardo Michelotto, Carossa Massimo, Perrone Letizia, Saratti Carlo Massimo, Rocca Giovanni Tommaso, Femiano Rossella, Femiano Felice, Scotti Nicola
| 期刊: | Materials | 影响因子: | 3.200 |
| 时间: | 2021 | 起止号: | 2021 Jul 14; 14(14):3920 |
| doi: | 10.3390/ma14143920 | ||
特别声明
1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。
2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。
3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。
4、投稿及合作请联系:info@biocloudy.com。