Failure Analysis of Ultra-High Molecular Weight Polyethylene Tibial Insert in Total Knee Arthroplasty.

全膝关节置换术中超高分子量聚乙烯胫骨垫片的失效分析

阅读:2
作者:Manescu Paltanea Veronica, Antoniac Iulian, Antoniac Aurora, Paltanea Gheorghe, Miculescu Marian, Bita Ana-Iulia, Laptoiu Stefan, Niculescu Marius, Stere Alexandru, Paun Costel, Cristea Mihai Bogdan
Knee osteoarthritis is treated based on total knee arthroplasty (TKA) interventions. The most frequent failure cause identified in surgical practice is due to wear and oxidation processes of the prothesis' tibial insert. This component is usually manufactured from ultra-high molecular weight polyethylene (UHMWPE). To estimate the clinical complications related to a specific prosthesis design, we investigated four UHMWPE tibial inserts retrieved from patients from Clinical Hospital Colentina, Bucharest, Romania. For the initial analysis of the polyethylene degradation modes, macrophotography was chosen. A light stereomicroscope was used to estimate the structural performance and the implant surface degradation. Scanning electron microscopy confirmed the optical results and fulfilled the computation of the Hood index. The oxidation process in UHMWPE was analyzed based on Fourier-transform infrared spectroscopy (FTIR). The crystallinity degree and the oxidation index were computed in good agreement with the existing standards. Mechanical characterization was conducted based on the small punch test. The elastic modulus, initial peak load, ultimate load, and ultimate displacement were estimated. Based on the aforementioned experimental tests, a variation between 9 and 32 was found in the case of the Hood score. The oxidation index has a value of 1.33 for the reference sample and a maximum of 9.78 for a retrieved sample.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。