Continuous ceramic fiber comprising silicon carbide-zirconium carbide (SiC-ZrC) binary phases was obtained through melt spinning, electron-beam curing and pyrolysis of a pre-ceramic precursor of polyzirconocenecarbosilanes (PZCS). After pyrolysis and heat treatment, ZrC particles with mean diameters of 15-20 nm were formed and homogeneously dispersed in a matrix of fine crystalline β-SiC with an average grain size of 6-10 nm. Concentration of Zr in the fiber varies from 14.88% to 17.45% by mass. Fibers consisting of near-stoichiometric ZrC and SiC with little free carbon can be obtained through pyrolysis decarbonization of the as-cured fiber in hydrogen from room temperature to 1000 °C, and subsequently heat treatment in argon up to 1600 °C for 1 h. High-temperature treatment of these amorphous inorganic fibers leads to crystallization of the binary phases of β-SiC and ZrC. The removal of free carbon under hydrogen results in more rapid growth of β-SiC and ZrC crystals, in which obvious aggregation of the dispersed ZrC particles among the continuous β-SiC matrix can be ascribed to a fast migration of Zr cation.
Microstructures of a SiC-ZrC Ceramic Fiber Derived from a Polymeric Precursor.
阅读:19
作者:Ge Min, Lv Xiaoxu, Zhang Hao, Yu Shouquan, Lu Zhenxi, Zhang Weigang
| 期刊: | Materials | 影响因子: | 3.200 |
| 时间: | 2020 | 起止号: | 2020 May 6; 13(9):2142 |
| doi: | 10.3390/ma13092142 | ||
特别声明
1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。
2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。
3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。
4、投稿及合作请联系:info@biocloudy.com。