Abstract

PURPOSE: The aim of this study was to investigate and compare the color stability of provisional restorative materials fabricated by 3D printing, dental milling, and conventional materials. MATERIALS AND METHODS: For the experimental groups, two commercially available 3D-printing provisional resins (E-Dent 100; EnvisionTEC GmbH, Germany & VeroGlaze™; Stratasys®, USA), two dental milling blocks (PMMA Disk; Yamahachi Dental Co., Japan & Telio®CAD; Ivoclar Vivadent AG, Liechtenstein), and two conventional materials (Alike™; GC Co., Japan & Luxatemp automix plus; DMG, Germany) were used. The water sorption and solubility test were (n=10, respectively) carried out according to ISO4049:2000 (International Standards Organization, Geneva, Switzerland). For the color stability test (n=10), coffee and black tea were used as staining solutions, and the specimens were stored for 12 weeks. Data were analyzed by one-way ANOVA and Tukey's HSD using SPSS version 22.0 (SPSS Inc. Chicago, IL, USA) (P<.05). RESULTS: Alike and Veroglaze showed the highest values and Luxatemp showed the lowest water sorption. In the color stability test, the ΔE of conventional materials varied depending on the staining solution. PMMA milling blocks showed a relatively low ΔE up to 4 weeks, and then significantly increased after 8 weeks (P<.05). 3D-printed materials exhibited a high ΔE or a significant increase over time (P<.05). CONCLUSION: The degree of discoloration increased with time, and a visually perceptible color difference value (ΔE) was shown regardless of the materials and solutions. PMMA milled and 3 D-printed materials showed more rapid change in discoloration after 8 weeks.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。