The effects of different surface treatments on the shear bond strengths of two dual-cure resin cements to CAD/CAM restorative materials

不同表面处理对两种双固化树脂粘接剂与CAD/CAM修复材料剪切粘接强度的影响

阅读:1

Abstract

PURPOSE: The aim of the present study was to investigate the effects of surface treatments on the bond strengths between polymer-containing restorative materials and two dual-cure resin cements. MATERIALS AND METHODS: In the present study, rectangular samples prepared from Lava Ultimate (LU) and Vita Enamic (VE) blocks were used. The specimen surfaces were treated using CoJet sandblasting, 50 µm Al(2)O(3) sandblasting, % 9 HF (hydrofluoric) acid, ER,Cr:YSGG laser treatment, and Z-Prime. Dual-cure resin cements (TheraCem and 3M RelyX U 200) were applied on each specimen's treated surface. A micro-tensile device was used to evaluate shear bond strength. Statistical analysis was performed using the SAS 9.4v3. RESULTS: While the bond strength using TheraCem with LU or VE was not statistically significant (P=.164), the bond strength using U200 with VE was statistically significant (P=.006). In the TheraCem applied VE groups, Z-Prime and HF acid were statistically different from CoJet, Laser, and Sandblast groups. In comparison of TheraCem used LU group, there was a statistically significant difference between HF acid and other surface treatments. CONCLUSION: The bonding performance between the restorative materials and cements were material type-dependent and surface treatment had a large effect on the bond strength. Within the limitations of the study, the use of both U200 and TheraCem may be suggested if Z-prime was applied to intaglio surfaces of VE. The cementation of LU using TheraCem is suitable after HF acid conditioning of the restoration surfaces.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。