Wear of primary teeth caused by opposed all-ceramic or stainless steel crowns

乳牙因对颌全瓷或不锈钢牙冠而磨损

阅读:2

Abstract

PURPOSE: This study was conducted to evaluate the effects of full-coverage all-ceramic zirconia, lithium disilicate glass-ceramic, leucite glass-ceramic, or stainless steel crowns on antagonistic primary tooth wear. MATERIALS AND METHODS: There were four study groups: the stainless steel (Steel) group, the leucite glass-ceramic (Leucite) group, the lithium disilicate glass-ceramic (Lithium) group, and the monolithic zirconia (Zirconia) group. Ten flat crown specimens were prepared per group; opposing teeth were prepared using primary canines. A wear test was conducted over 100,000 chewing cycles using a dual-axis chewing simulator and a 50 N masticating force, and wear losses of antagonistic teeth and restorative materials were calculated using a three-dimensional profiling system and an electronic scale, respectively. Statistical significance was determined using One-way ANOVA and Tukey's test (P<.05). RESULTS: The Leucite group (2.670±1.471 mm(3)) showed the greatest amount of antagonist tooth wear, followed by in decreasing order by the Lithium (2.042±0.696 mm(3)), Zirconia (1.426±0.477 mm(3)), and Steel groups (0.397±0.192 mm(3)). Mean volume losses in the Leucite and Lithium groups were significantly greater than in the Steel group (P<.05). No significant difference was observed between mean volume losses in the Zirconia and Steel groups (P>.05). CONCLUSION: Leucite glass-ceramic and lithium disilicate glass-ceramic cause more primary tooth wear than stainless steel or zirconia.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。