A Simple, Safe, and Effective Method for Preparing Autologous Bio-Based Fibrin Glue for Ophthalmic Use

一种简单、安全、有效的眼科用自体生物基纤维蛋白胶制备方法

阅读:11
作者:Luis Fernández-Vega-Cueto, Mairobi Persinal-Medina, Natalia Vázquez, Manuel Chacón, Belén Alfonso-Bartolozzi, Sergio Alonso-Alonso, Teresa Sánchez, Silvia Berisa-Prado, Laura María Martínez-López, Jesús Merayo-Lloves, Álvaro Meana

Abstract

This study proposes a method to prepare autologous bio-based fibrin glue (FG) for use in ophthalmic surgery. FGs containing three fibrinogen concentrations and a thrombin concentrate were prepared using human blood from five donors (FG1: physiological fibrinogen concentration; FG2 and FG3: concentrated fibrinogen). The adhesion strength was tested, and the clinical safety and efficacy were studied in rabbit eyes in conjunctival surgery. A commercial FG was used as a control. From each donor, 2 mL of FG was prepared, containing 1 mL of 3.49 ± 0.78 (FG1), 17.74 ± 4.66 (FG2), or 47.46 ± 9.36 mg/mL (FG3) of fibrinogen and 1 mL of 2248.12 ± 604.20 UI/mL of thrombin. The average adhesion strength increased with the fibrinogen concentration, from 1.49 ± 0.39 kPa (FG1) to 3.14 ± 1.09 kPa (FG3). FG1 showed poor results when used for autograft adhesion. In contrast, the conjunctival autografts were successfully grafted using FG2 and FG3, revealing equivalent adhesion properties compared with commercial FG, but with less inflammation. In conclusion, FGs could be prepared on demand within minutes from small volumes of human blood, using a method that results in FGs which exhibit good adhesion capacity and are also safe and effective in a preclinical study.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。