Ion release from a composite resin after exposure to different 10% carbamide peroxide bleaching agents

复合树脂暴露于不同浓度的10%过氧化脲漂白剂后离子的释放

阅读:1

Abstract

OBJECTIVE: This in vitro study evaluated the influence of two 10% carbamide peroxide bleaching agents - a commercial product (Opalescence PF; Ultradent Products, Inc.) and a bleaching agent prepared in a compounding pharmacy - on the chemical degradation of a light-activated composite resin by determining its release of ions before and after exposure to the agents. MATERIAL AND METHODS: Thirty composite resin (Filtek Z250; 3M/ESPE) samples were divided into three groups: group I (exposed to Opalescence PF commercial bleaching agent), group II (exposed to a compounded bleaching agent) and group III (control - Milli-Q water). After 14 days of exposure, with a protocol of 8 h of daily exposure to the bleaching agents and 16 h of immersion in Milli-Q water, the analysis of ion release was carried out using a HP 8453 spectrophotometer. The values were analyzed statistically by ANOVA, Tukey's test and the paired t-tests. The significance level was set at 5%. RESULTS: After 14 days of the experiment, statistically significant difference was found between group II and groups I and III, with greater ion release from the composite resin in group II. CONCLUSIONS: The compounded bleaching agent had a more aggressive effect on the composite resin after 14 days of exposure than the commercial product and the control (no bleaching).

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。