Depth of cure of dental composites submitted to different light-curing modes

不同光固化模式下牙科复合材料的固化深度

阅读:1

Abstract

OBJECTIVE: This study evaluated the depth of cure of five dental composites submitted to different light-curing modes. MATERIAL AND METHODS: Canal-shaped cavities with 5mm of length were prepared on the buccal surfaces of extracted third molars, and restored using P-60, A-110, Admira, Z-250 and Supreme resin composites. Materials were light-cured from the top, according to three modes (Group 1- Conventional (C): 500 mW/cm(2) / 40 s; Group 2 - Soft-Start (SS): 250 mW/cm(2)/ 20 s + 500 mW/cm(2)/ 20 s + 500 mW/cm(2)/ 10 s and Group 3 - LED: 250 mW/cm(2)/ 40 s). After that, cavity longitudinal surfaces were polished and marked with a millimeter scale of 4mm of length. Depth of cure was evaluated by means of Knoop hardness number (KHN), so that five indentations were performed at each millimeter. Original data were submitted to three-way ANOVA and Fisher's LSD test (alpha = 0.01). RESULTS: All materials presented a significant reduction on KHN from first to third millimeter. Regarding depth of cure, the results obtained for Conventional and Soft-Start modes were similar, but statistically superiors to those found for group 3 (LED). CONCLUSION: This performance may be related to the differences among energy densities obtained with different light-curing modes.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。