The effect of vancomycin addition to the compression strength of antibiotic-loaded bone cements

万古霉素的添加对载药骨水泥抗压强度的影响

阅读:1

Abstract

The purpose of this study was to record the effect of the addition of vancomycin on the compression strength of antibiotic-loaded bone cement and to compare the results with the international standards (ISO 5833-2). The formulations tested were: Palamed G and Copal. Vancomycin concentrations of 2.5%, 5% and 10% per powder weight were added. Samples of Palamed G with 5% vancomycin and non-standardised mixing procedures were also tested. The ISO requirements for the testing procedures were followed. None of the combinations tested fall short of the ISO standards for compression strength. Copal with 10% and Palamed G with 5% vancomycin and non-standardised mixing procedures, however, did not significantly exceed them. The addition of up to 5% vancomycin per powder weight to the Palamed G and Copal bone cements can be considered safe. Care should be given to the mixing procedure of the cement, as it significantly affects its compression strength.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。