OBJECTIVE: To assess the enamel surface damage and residual adhesive remnant [adhesive remnant index (ARI)] on extracted premolars after debonding the ceramic brackets using three different debonding techniques, with optical coherence tomography (OCT). METHODS: Ninety extracted premolars were bonded with ceramic brackets and divided into three groups of 30 teeth each based on debonding techniques used. Twenty-four hours later, they were debonded using three different debonding techniques: debonding pliers, ultrasonic scalers, and Er-YAG laser. A baseline scan was obtained prior to bonding using OCT. The teeth were evaluated for the adhesive remnant on the tooth surface using ARI score, and the amount of enamel surface damage was evaluated using OCT. RESULTS: We observed that the use of ultrasonic scalers as a debonding technique led to greater incidence of enamel surface damage as measured in OCT. The ARI scores with debonding pliers and laser were significantly greater than that of scaler debonding. CONCLUSIONS: Results of this in vitro study confirmed that use of ultrasonic scalers as a debonding technique led to significantly greater incidence of enamel surface damage when compared to the other two debonding techniques. The ARI scores on the tooth surface using debonding pliers and laser were significantly greater than that of the scaler debonding technique.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。