Fracture load of chairside CAD-CAM veneers fabricated with pre-and fully crystalized lithium disilicate ceramics

采用预结晶和全结晶二硅酸锂陶瓷制成的椅旁CAD-CAM贴面的断裂载荷

阅读:2

Abstract

PURPOSE: To evaluate the fracture load of chairside computer-aided design and computer-aided manufacturing (CAD-CAM) veneers fabricated with two conventional pre-crystallized and two fully crystallized lithium disilicate ceramic materials. MATERIALS AND METHODS: Seventy-five chairside CAD-CAM veneers (15 specimens/group) for maxillary right central incisors were fabricated with different lithium disilicate brands: (1) IPS e.max CAD; (2) Amber Mill; (3) Cerec Tessera; (4) n!ce Straumann; and (5) GC Initial LiSi Block. Restorations were cemented with resin luting cement (Variolink Esthetic, Ivoclar) to 3D-printed resin dies. Bonded restorations received 5000 thermal cycles and then were loaded until fracture. Statistical analysis included One-Way ANOVA. RESULTS: Conventional pre-crystallized e.max CAD displayed the highest fracture load value (640 N), followed by fully-crystallized n!ce Straumann (547 N), pre-crystallized Cerec Tessera (503 N), pre-crystallized Amber Mill (476 N), respectively; fully-crystallized GC Initial LiSi Block (431 N) displayed the lowest values. When comparing the fracture load of recent lithium disilicate ceramic material to the e.max group, which acted as the control, significant differences were noted. The LiSi Block GC group, in particular, had considerably higher mean difference values (208.867, p < 0.001, 95% CI [89.63, 328.10]), as did the Amber Mill group (164.200, p = 0.002, 95% CI [44.96, 283.44]) and CEREC Tessera group (137.533, p = 0.016, 95% CI [18.30, 256.77]). The e.max and n!ce Straumann groups had no statistically significant differences in mean scores (92.933, p = 0.198, 95% CI [-26.30, 212.17]). These findings imply that the clinical performance of recent lithium disilicate veneers varies when compared to the e.max CAD group. CONCLUSIONS: The fracture load of chairside CAD-CAM lithium disilicate veneers for maxillary central incisors varies according to the type of ceramic brands. Conventional pre-crystallized e.max CAD displayed higher fracture load than the recent pre- and fully-crystallized lithium disilicate materials, emphasizing the significance of choosing the right product based on the desired clinical outcome.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。