Color Stability of Resin Hybrid Ceramic Materials in Comparison to Zirconia-Reinforced Lithium Silicate Ceramic

树脂混合陶瓷材料与氧化锆增强硅酸锂陶瓷的颜色稳定性比较

阅读:1

Abstract

Objectives: This in vitro study aimed to compare the effect of external staining agents (black tea and grape juice) on the color change of three hybrid ceramics including a new material in comparison to zirconia-reinforced lithium silicate. Materials and Methods: Ten samples of two hybrid dental ceramics including Vita Enamic (Vita Zahnfabrik) and Crystal Ultra (Digital Dental) in addition to a resin nanoceramic, Lava Ultimate (3M ESPE); and a zirconia-reinforced lithium silicate glass ceramic, Vita Suprinity (Vita Zahnfabrik) were prepared and immersed in black tea or grape juice for 30 days. A spectrophotometer was used to evaluate color change. All samples were carefully chosen in A3 shades or their equivalent. Two-way ANOVA and Bonferroni tests were used to analyze the color differences (ΔE00) among the materials and the staining solutions at a significant level of 0.05. Results: Significant color changes were observed in Vita Enamic and Lava Ultimate groups after immersion in both solutions (P<0.001). The least color changes (ΔE00) belonged to the Vita Suprinity (1.34) and Crystal Ultra (1.92) groups, respectively. Conclusion: The color changes of Vita Enamic and Lava Ultimate materials were beyond clinical acceptability. However, the mean color changes of Vita Suprinity and Crystal Ultra groups were clinically acceptable.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。