Effect of Thickness on Fluorescence of Some Clinical Dental Ceramics

厚度对某些临床牙科陶瓷荧光的影响

阅读:1

Abstract

Objectives: This study aimed to develop a new method for measurement of florescence and compare the fluorescence of some clinical dental ceramics in different thicknesses. Materials and Methods: Forty-eight samples of feldspathic (Vita VM9, A2), IPS e.max (Ivoclar HT, A2), zirconia (Korox Zircostar, A2) and Enamic (Vita A2) ceramics were used in this study in 0.5 and 1 mm thicknesses. The fluorescence of the samples was measured by using a developed technique. The results were analyzed by two-way ANOVA and Duncan post-hoc test. P<0.05 was considered significant. Results: Enamic, feldspathic and e.max ceramics had significantly different fluorescence in descending order (P=0.000). Fluorescence of ceramics increased with an increase in their thickness from 0.5 to 1 mm (P=0.007). Conclusion: The results confirmed the applicability of the presented method for measurement of fluorescence of dental ceramics. While, the thickness of restoration determines the concentration of the fluorescent agent, some additional technical information is required for justification of the observed trend in the studied ceramics.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。