Color stability of esthetic restorative materials: a spectrophotometric analysis

美学修复材料的颜色稳定性:分光光度分析

阅读:1

Abstract

Objective: The aim of this in vitro study was to evaluate the color stability of different restorative materials (one microfilled composite, one nanofilled composite, one nanohybrid composite and one Ormocer-based composite) after exposure to different staining solutions (coffee, coca-cola and red wine). Material and methods: All materials were polymerized into silicon rings (2 mm ×6 mm ×8 mm) to obtain specimens identical in size. Thirty cylindrical specimens of each material were prepared. They were immersed in staining solutions over a 28-day test period. A colorimetric evaluation according to the CIE L*a*b* system was performed by a blind trained operator at 7, 14, 21, 28 days of the staining process. The Shapiro-Wilk test and Kruskal-Wallis ANOVA were applied to assess significant differences among restorative materials. The paired t-test was applied to test which CIE L*a*b* parameters significantly changed after immersion in staining solutions. Results: All restorative materials showed clinically perceptible color differences after immersion in coffee. L* and b* values showed the highest variability. Coca cola and red wine did not influence the color stability for all restorative materials except for Filtek Supreme XTE. Conclusions: Coffee caused a significant color change in all types of tested composite resins. Filtek Supreme XTE demonstrated alone a staining susceptibility to red wine; no other significant differences among the materials were demonstrated. Long-term exposure to some food dyes (coffee in particular) can significantly affect the color stability of modern esthetic restorative materials regardless of materials' different composition.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。