Long-Term Water Balance Evaluation in Glass Ionomer Restorative Materials

玻璃离子修复材料的长期水分平衡评估

阅读:1

Abstract

The complex role of water in glass ionomer cement (polyalkenoate) dental restorative materials has been studied, but much of the present understanding concerning water balance within these materials is based on very early studies and short-term experiments. This study evaluated the nature of the water species of six conventional and four resin modified glass ionomer restorative materials over 3 years using thermogravimetric analysis techniques. Materials were prepared, placed in crucibles, and stored in physiologic phosphate buffered saline and evaluated at 24 h, 1 week, and then at 1, 3, 6, 9, 12, 18, 24, 30 and 36 months. All materials demonstrated a significant increase in unbound water percentage content but except for the resin modified materials, the enthalpy required to remove the unbound water species did not significantly change over 36 months. Also, bound water content percentage and removal enthalpy was established at 24 h, as no significant increase was noted in both bound water content and removal enthalpy over the course of this evaluation. This study suggests that unbound water species may increase with time and is loosely held except for the resin modified materials. Protective coatings placement and re-evaluation are prudent to prevent unbound water loss.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。