Evaluating the Wear of Resin Teeth by Different Opposing Restorative Materials

评估不同对颌修复材料对树脂牙的磨损情况

阅读:1

Abstract

The aim of this study was to evaluate the wear properties of resin teeth with different opposing dental restorative materials. One type of resin tooth (Trubyte Biotone) was tested against six types of restorative materials including type III gold alloy (GO), monolithic zirconia (MZ), lithium disilicate glass ceramic (LD), nickel-chromium alloy (NC), feldspathic ceramic (FC), and steatite (ST). Two-body wear tests were performed under a vertical load of 5 kgf and thermo-cycling at 5/55 °C with a total of 120,000 cycles. The wear amount was quantified by measuring the volume loss of the resin teeth and the vertical substance loss of the opposing materials using three-dimensional images. The FC group showed a significantly greater amount of wear of the resin teeth, followed by the ST, NC, LD, MZ, and GO groups. The GO group showed significantly less wear of resin teeth than the other groups. There were no statistically significant differences in the wear of opposing restorative materials between groups. Within the limits of this study, it is recommended that zirconia, rather than feldspathic ceramic, should be used for restorations in the esthetic zone, and gold alloy should be used for areas with little or no esthetic demand.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。