Synthesis of Isohexide Diyne Polymers and Hydrogenation to Their Saturated Polyethers

异己二炔聚合物的合成及其氢化得到饱和聚醚

阅读:1

Abstract

The incorporation of renewable feedstocks into polymer backbones is of great importance in modern polymer science. We report the synthesis of 1,3-diyne polymers derived from the bispropargyl ethers of isosorbide, isomannide, and isoidide. The dialkyne monomers can be polymerized through an adaptation of the Glaser-Hay coupling using a nickel(II) cocatalyst. These well-defined diyne polymers bear an iodoalkyne end group, afforded through an unanticipated reductive elimination pathway, and display glass transition temperatures (T(g)) from 55 to 64 °C. Fully saturated, analogous polyethers can be prepared from the hydrogenation of the diyne polymers, and these show T(g) values between -10 and -2 °C. Both the 1,3-diyne polymers and the saturated analogues display similar trends in their T(g) values vis-à-vis the stereochemical features of the isohexide unit within the backbone. This polymerization provided access to two series of isohexide-based polyethers, the thermal properties of which are influenced by the nature of the 2,4-hexadiynyl and hexamethylene linkers as well as the relative configuration of the bicyclic subunit in the backbone. The reported method represents an important step toward accessing well-defined polyethers from renewable feedstocks using readily available catalysts and convenient ambient conditions.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。