Facile Preparation of a Transparent, Self-Healing, and Recyclable Polysiloxane Elastomer Based on a Dynamic Imine and Boroxine Bond

基于动态亚胺和硼氧烷键的透明、自修复、可回收聚硅氧烷弹性体的简易制备

阅读:7
作者:Peng Wang, Zhuochao Wang, Wenxin Cao, Jiaqi Zhu

Abstract

Transparent polysiloxane elastomers with good self-healing and reprocessing abilities have attracted significant attention in the field of artificial skin and flexible displays. Herein, we propose a simple one-pot method to fabricate a room temperature self-healable polysiloxane elastomer (HPDMS) by introducing dynamic and reversible imine bonds and boroxine into polydimethylsiloxane (PDMS) networks. The presence of imine bonds and boroxine is proved by FT-IR and NMR spectra. The obtained HPDMS elastomer is highly transparent with a transmittance of up to 80%. The TGA results demonstrated that the HPDMS elastomer has good heat resistance and can be used in a wide temperature range. A lower glass transition temperature (Tg, -127.4 °C) was obtained and revealed that the elastomer is highly flexible at room temperature. Because of the reformation of dynamic reversible imine bonds and boroxine, the HPDMS elastomers exhibited excellent autonomous self-healing properties. After healing for 3 h, the self-healing efficiency of HPDMS reached 96.3% at room temperature. Moreover, the elastomers can be repeatedly reprocessed multiple times under milder conditions. This work provides a simple but effective method to prepare transparent self-healable and reprocessable polysiloxane elastomers.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。