Enhanced Storage Stability of Different Polymer Modified Asphalt Binders through Nano-montmorillonite Modification

通过纳米蒙脱石改性提高不同聚合物改性沥青粘合剂的储存稳定性

阅读:1

Abstract

The storage stability concern, caused by phase separation for the density difference between polymers and asphalt fractions, has limited the widespread application of polymer modified asphalt (PMA). Therefore, this study aims to improve the storage concern of PMA by incorporating nano-montmorillonite. To this end, different nano-montmorillonites were incorporated to three PMAs modified with three typical asphalt modifiers, i.e., crumb rubber (CRM), styrene-butadiene-rubber (SBR) and styrene-butadiene-styrene (SBS). A series of laboratory tests were performed to evaluate the storage stability and rheological properties of PMA binders with nano-montmorillonite. As a consequence, the incorporation of nano-montmorillonite exhibited a remarkable effect on enhancing the storage stability of the CRM modified binder, but limited positive effects for the SBR and SBS modified binders. The layered nano-montmorillonite transformed to intercalated or exfoliated structures after interaction with asphalt fractions, providing superior storage stability. Among selected nano-montmorillonites, the pure montmorillonite with Hydroxyl organic ammonium performed the best on enhancing storage stability of PMA. This paper suggests that nano-montmorillonite is a promising modifier to alleviate the storage stability concern for asphalt with polymer modifiers.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。