Radiation and mechanical performance of cementitious materials containing ecofriendly nano laboratory waste glass

含环保纳米实验室废玻璃水泥基材料的辐射和力学性能

阅读:1

Abstract

This study helps in managing waste glass and greening the environment by incorporating laboratory waste glass into mortar production to make an eco-friendly shielding material against gamma rays. The efficiency of using waste glass powder as a cement replacement or addition in mortar production was studied by using two waste glass sizes: micro glass (particle size range from 10.09 to 24.73 μm) and nano glass (particle size range from 10.57 to 26.42 nm) to design different mortar specimens with varying percentages of fine glass powder from 0 to 30%. Compressive strength and flexure strength were evaluated to determine mechanical properties. The results indicated that adding WGP to mortar positively affects the characteristics of cementitious composites. The linear and mass attenuation coefficients of the samples were experimentally determined using a NaI detector and various radioactive sources (Am-241, Ba-133, Eu-152, Cs-137, and Co-60) with gamma energies ranging from 59.53 to 1332 keV. The obtained coefficients were then compared to the theoretical values of the composites using XCOM software to verify their accuracy. Additionally, the half-value layer, tenth-value layer, mean free path, and effective atomic number were computed. Furthermore, the results revealed that the mortar sample with 30% nano additive glass was the most effective in reducing gamma radiation.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。