Surface roughness and erosion of nanohybrid and nanofilled resin composites after immersion in red and white wine

纳米混合和纳米填充树脂复合材料浸泡在红葡萄酒和白葡萄酒后的表面粗糙度和侵蚀情况

阅读:1

Abstract

AIMS: This study aimed to investigate the effects of red and white wine on the surface roughness and erosion of nanohybrid and nanofilled resin composites. MATERIALS AND METHODS: Sixty specimens of each resin-based composite (RBC) were prepared. Before immersion, baseline data roughness values were recorded using a profilometer. Three groups of discs (n = 20) were then alternately immersed in red wine, white wine, and deionized water (as a control) for 25 min and artificial saliva for 5 min over four cycles. The specimens were then stored in artificial saliva for 22 h. This process was repeated for 5 days following immersion in artificial saliva for 2 days. Subsequently, the process was repeated. After immersion, the specimens were evaluated and data were analyzed by two-way repeated analysis of variance (ANOVA) and Tukey's honestly significant difference (HSD) (α = 0.05). RESULTS: Red wine caused significantly greater roughness and erosion than did white wine and deionized water (P < 0.05). Nanohybrid resin composites were significantly rougher than nanofilled resin composites (P < 0.05). CONCLUSION: The effects of red and white wine on the surface roughness and erosion of resin composite restorative materials depended upon the physical and chemical composition of the restorative materials and the types of wine.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。