Effect of acidic environment on color and translucency of different indirect restorative materials

酸性环境对不同间接修复材料颜色和透明度的影响

阅读:1

Abstract

PURPOSE: The aim of the current study was to evaluate the effect of simulated gastric acid on the color and translucency of different indirect restorative materials. MATERIALS AND METHODS: A total of 36 disc-shaped samples were cut by using an isomet saw and divided into four equal groups (n = 9) according to the material type: Group Z: translucent zirconia (Ceramill® Zolid ht.(+) preshade, Amann Girrbach, Koblach, Austria); Group E: lithium disilicate (IPS e.max CAD, Ivoclar Vivadent AG, Schaan, Liechtenstein); Group C: resin nanoceramic (Cerasmart, GC, Tokyo, Japan); Group P: polyether ether ketone (PEEK) (Bettin Zirconia Dentale Italy) veneered with indirect high impact polymer composite (HIPC) (breCAM HIPC, Bredent GmbH & Co. KG, Germany). The samples were immersed in simulated gastric acid (HCl, pH 1.2) for 96 hours at 37 °C in an incubator. The color change (ΔE(00)) and translucency (RTP(00)) were measured every 9.6 hours (one-year clinical simulation) of immersion in simulated gastric acid. RESULTS: For color change (∆E(00)) and translucency (RTP(00)) among the tested materials, there was a highly statistically significant difference (P < 0.001) after every year of follow-up. The color change in both Z and G groups was the lowest after 1 year of acid immersion, followed by that in group H, and the highest change in color was recorded in group P. CONCLUSION: High translucent zirconia is recommended in patients who are concerned about esthetic, especially with acidic oral environment.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。