In vitro surface and color changes of tooth-colored restorative materials after sport and energy drink cyclic immersions

运动和能量饮料循环浸泡后牙色修复材料的体外表面和颜色变化

阅读:1

Abstract

BACKGROUND: There has not been any research conducted on surface properties and color changes from sport and energy drinks on bulk-fill resin composite, nanohybrid resin composite and glass ionomer restorative material. The aim of this in vitro study was to investigate the effect of sport and energy drinks on surface hardness, roughness and color changes of bulk-fill resin composite, nanohybrid resin composite and glass ionomer restorative material, and to also evaluate the acidity and titratable acidity of the drinks. METHODS: One hundred and forty-seven specimens of each tooth-colored restorative material were prepared in a polytetrafluoroethylene mold (10 mm. in diameter and 2 mm. in thickness). Before immersion, baseline data of hardness, roughness, and color value were recorded. Each material was divided into 3 groups for sport drink, energy drink, and deionized water (serving as a control). The specimens were immersed in a storage agent for 5 s, then in artificial saliva for 5 s alternately for 24 cycles, and then stored in artificial saliva for 24 h. The immersion cycle was repeated for 14 days and hardness, roughness and color values were measured at 7 and 14 days. RESULTS: After immersion, the glass ionomer restorative material had statistically less hardness, more roughness and more color changes than the others (P < 0.05). Energy drink groups statistically caused more surface and color changes than sport drink groups (P < 0.05). CONCLUSION: Sport and energy drinks affected hardness, roughness, and color changes in all the tooth-colored restorative materials evaluated.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。