Decellularization compromises mechanical and structural properties of the native trachea

脱细胞化损害天然气管的机械和结构特性

阅读:12
作者:Allison M Greaney, Abhay B Ramachandra, Yifan Yuan, Arina Korneva, Jay D Humphrey, Laura E Niklason

Abstract

Tracheal replacement using tissue engineering technologies offers great potential to improve previously intractable clinical interventions, and interest in this area has increased in recent years. Many engineered airway constructs currently rely on decellularized native tracheas to serve as the scaffold for tissue repair. Yet, mechanical failure leading to airway narrowing and collapse remains a major cause of morbidity and mortality following clinical implantation of decellularized tracheal grafts. To understand better the factors contributing to mechanical failure in vivo, we characterized the histo-mechanical properties of tracheas following two different decellularization protocols, including one that has been used clinically. All decellularized tracheas deviated from native mechanical behavior, which may provide insights into observed in vivo graft failures. We further analyzed protein content by western blot and analyzed microstructure by histological staining and found that the specific method of decellularization resulted in significant differences in the depletion of proteoglycans and degradation of collagens I, II, III, and elastin. Taken together, this work demonstrates that the heterogeneous architecture and mechanical behavior of the trachea is severely compromised by decellularization. Such structural deterioration may contribute to graft failure clinically and limit the potential of decellularized native tracheas as viable long-term orthotopic airway replacements.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。