In Vitro Comparison to Evaluate Metal Ion Release: Nickel-Titanium vs. Titanium-Molybdenum Orthodontic Archwires

体外比较评估金属离子释放:镍钛合金与钛钼合金正畸弓丝

阅读:1

Abstract

Background When metals used in orthodontic materials are exposed to the oral environment, teeth, and gingivae over an extended period of time, they may gradually deteriorate. As a result, the patient is exposed to higher concentrations of metals and metal ions than what they would be exposed to through food and other sources. The goal of the current in vitro experiment was to evaluate and contrast the metal ion release from orthodontic archwires made of titanium-molybdenum alloy (TMA) and nickel-titanium (NiTi). Methods For 90 days, 20 orthodontic archwires in each group were immersed in 50 milliliters of simulated saliva using different containers. Atomic Absorption Spectrometry (AAS) (Shimadzu Corporation, Kyoto, Japan) was used to assess and compare metal ion emission. The unit of measurement is parts per million (PPM). Results The findings indicated that the discharge of nickel metal from the NiTi archwire (Group A) was much higher than that from the TMA archwire (Group B), with a statistical significance level of p < 0.001. It was discovered that Group B's release of titanium was statistically significantly (p < 0.05) higher than Group A's titanium release, which did not include the release of any other metals. Conclusion The study findings indicated that the amounts of metal ions released from the orthodontic archwires made of titanium molybdenum and nickel-titanium alloy were within safety limits.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。