Biological behavior exploration of a paclitaxel-eluting poly-l-lactide-coated Mg-Zn-Y-Nd alloy intestinal stent in vivo

在体内探索紫杉醇洗脱聚乳酸涂层Mg-Zn-Y-Nd合金肠支架的生物学行为

阅读:1

Abstract

As a new type of intestinal stent, the MAO/PLLA/paclitaxel/Mg-Zn-Y-Nd alloy stent has shown good degradability, although its biocompatibility in vitro and in vivo has not been investigated in detail. In this study, its in vivo biocompatibility was evaluated by animal study. New Zealand white rabbits were implanted with degradable intestinal Mg-Zn-Y-Nd alloy stents that were exposed to different treatments. Stent degradation behavior was observed both macroscopically and using a scanning electron microscope (SEM). Energy dispersion spectrum (EDS) and histological observations were performed to investigate stent biological safety. Macroscopic analysis showed that the MAO/PLLA/paclitaxel/Mg-Zn-Y-Nd stents could not be located 12 days after implantation. SEM observations showed that corrosion degree of the MAO/PLLA/paclitaxel/Mg-Zn-Y-Nd stents implanted in rabbits was significantly lower than that in the PLLA/Mg-Zn-Y-Nd stent group. Both histopathological testing and serological analysis of in vivo biocompatibility demonstrated that the MAO/PLLA/paclitaxel/Mg-Zn-Y-Nd alloy stents could significantly inhibit intestinal tissue proliferation compared to the PLLA/Mg-Zn-Y-Nd alloy stents, thus providing the basis for designing excellent biodegradable drug stents.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。