Chromium(III) and chromium(VI) release from leather during 8 months of simulated use

模拟使用8个月期间皮革中铬(III)和铬(VI)的释放

阅读:1

Abstract

BACKGROUND: Chromium (Cr) release from Cr-tanned leather articles is a major cause of Cr contact dermatitis. It has been suggested that Cr(VI) release from leather is not necessarily an intrinsic property of the leather, but is strongly dependent on environmental conditions. OBJECTIVES: To test this hypothesis for long-term (8 months) simulated use. MATERIALS AND METHODS: The release of total Cr and Cr(VI) from Cr-tanned, unfinished leather was analysed in subsequent phosphate buffer (pH 8.0) immersions for a period of 7.5 months. The effect of combined ultraviolet treatment and alkaline solution (pH 12.1) was tested. Dry storage [20% relative humidity (RH)] was maintained between immersions. Atomic absorption spectroscopy, X-ray fluorescence and diphenylcarbazide tests were used. RESULTS: Cr(VI) release was dependent on previous dry storage or alkaline treatment, but not on duration or number of previous immersions. Cr(III) release decreased with time. Fifty-two percent of the total Cr released during the last immersion period was Cr(VI). Cr(VI) release exceeded 9 mg/kg in all immersion periods except in the first 10-day immersion (2.6 mg/kg). CONCLUSIONS: Cr(VI) release is primarily determined by environmental factors (RH prior to immersion, solution pH, and antioxidant content). The RH should be kept low prior to testing Cr(VI) release from leather.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。