Synergistic Impact of Alloying with Ni on Cu Cathode Interfaces for Fluoride Batteries

镍合金化对氟化物电池铜正极界面的协同效应

阅读:1

Abstract

All-solid-state fluoride batteries have the potential to achieve energy densities significantly higher than those of lithium-ion batteries. A common cathode material for fluoride batteries is Cu. Cu has a low polarization, but its rapid capacity degradation due to grain growth and subsequent delamination from the solid-state electrolyte are critical issues. To enhance the performance of Cu-based cathodes in all-solid-state fluoride batteries, we explore alloying of Cu with Ni to create metastable solid solution phases (Cu(x)Ni(1-x) with x = 0, 0.32, 0.52, 0.72, 0.89, and 1.0). Compared to Cu, Ni has a higher polarization but exhibits superior capacity retention. The Cu(0.72)Ni(0.28) alloy demonstrates a polarization as low as Cu, but it has a significantly improved capacity retention, which is comparable to Ni. Transmission electron microscopy observations demonstrate that the thin Ni-rich region formed near the interface inhibits Cu grain growth and delamination from the LaF(3) electrolyte. By incorporating an appropriate amount of Ni into Cu, Cu-Ni alloy films combine the advantages of both metals, improving the performance of fluoride batteries.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。