The use of bovine-derived hydroxyapatite xenograft for defect filling in opening-wedge high tibial osteotomy

牛源羟基磷灰石异种移植材料在开放楔形高位胫骨截骨术缺损填充中的应用

阅读:1

Abstract

High tibial osteotomy is a reliable procedure for the correction of knee varus deformity. An opening-wedge high tibial osteotomy (OW-HTO) is the most popular technique. The results of the bone defect after opening the wedge needed special treatment to ensure bone healing. This study aims to evaluate the use of bovine-derived hydroxyapatite graft for defect filling after OW-HTO. METHODS: A retrospective study was performed on all patients who received OW-HTO at Prof. Dr R. Soeharso Orthopaedic Hospital from November 2019 to December 2022. A total of 21 patients (24 knees) were included in this study. Clinical dan radiological evaluation was performed on all patients preoperative and postoperatively. The mean of the follow-up period was 12.6 months with a minimum of 4 months follow-up. RESULTS: Primary medial uni-compartment knee osteoarthritis was the most common diagnosis, with 17 of 24 cases (70.8%). Mechanical axis deviation was changed from 31 mm medial deviation (range: 8-52 mm) to 0.45 mm medial deviation (range: 13 - (-8) mm). The anatomic tibiofemoral angle was corrected from a preoperative mean of 4.7(°) of varus to a mean of 5.8(°) of valgus postoperatively. Bone defect height was mean 15.9 mm with a range of 10-23 mm. Bone defect width was mean 46.7 mm (range: 34-60 mm). Hydroxyapatite graft integration with the host bone was found in all patients during the final follow-up period. CONCLUSIONS: Bovine-derived hydroxyapatite graft is a safe and effective material for bone defect filling in OW-HTO procedures with a high bone union rate.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。