Porous Structure Enhances the Longitudinal Piezoelectric Coefficient and Electromechanical Coupling Coefficient of Lead-Free (Ba(0.85)Ca(0.15))(Zr(0.1)Ti(0.9))O(3)

多孔结构增强了无铅(Ba(0.85)Ca(0.15))(Zr(0.1)Ti(0.9))O(3)的纵向压电系数和机电耦合系数

阅读:1

Abstract

The introduction of porosity into ferroelectric ceramics can decrease the effective permittivity, thereby enhancing the open circuit voltage and electrical energy generated by the direct piezoelectric effect. However, the decrease in the longitudinal piezoelectric coefficient (d(33)) with increasing porosity levels currently limiting the range of pore fractions that can be employed. By introducing aligned lamellar pores into (Ba(0.85)Ca(0.15))(Zr(0.1)Ti(0.9))O(3), this paper demonstrates an unusual 22-41% enhancement in the d(33) compared to its dense counterpart. This unique combination of high d(33) and a low permittivity leads to a significantly improved voltage coefficient (g(33)), energy harvesting figure of merit (FoM(33)) and electromechanical coupling coefficient ( k332 ). The underlying mechanism for the improved properties is demonstrated to be a synergy between the low defect concentration and high internal polarizing field within the porous lamellar structure. This work provides insights into the design of porous ferroelectrics for applications related to sensors, energy harvesters, and actuators.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。