The effect of simulating body fluid on the structural properties of hydroxyapatite synthesized in the presence of citric acid

模拟体液对柠檬酸合成羟基磷灰石结构性质的影响

阅读:9
作者:Omer Kaygili, Serhat Keser, Mustafa Kom, Niyazi Bulut, Sergey V Dorozhkin

Abstract

In present work, the effect of citric acid (CA) addition in different amounts (0, 1, 5 and 10 ml) on the structure of hydroxyapatite (HAp) was investigated using X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) spectroscopy techniques. The crystallite dimensions, lattice parameters, unit cell volume, crystallinity percentage and Ca/P molar ratio were found to be affected by the CA content. To investigate the influence of CA on the bioactive properties of the HAp samples and to determine the optimum amount of CA, in vitro soaking tests in simulated body fluid (SBF) were performed. Although the samples' morphology was found to be affected by neither the amount of CA nor the soaking time in SBF, the soaking results revealed that the maximum changes in the Ca/P ratio were found for the HAp samples prepared in the presence of the highest amounts of CA, which pointed out to the highest bioactivity of these samples.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。