Effect of an Effervescent Multivitamin on Color and Surface Roughness of Micro-Hybrid Dental Resin Composites

泡腾复合维生素对微混合牙科树脂复合材料颜色和表面粗糙度的影响

阅读:1

Abstract

The use of multivitamins has become widespread globally, yet there is a scarcity of studies investigating their impact on resin composite restorations. This study aimed to evaluate the effect of an effervescent multivitamin tablet on micro-hybrid dental resin composites' surface roughness and color. Fifty disc-shaped samples (8 × 2 mm, shade A2; n = 10) were prepared and polished using five different micro-hybrid resin composites (Pergamon, Dentac, Turkey; Estelite Posterior, Tokuyama, Japan; Geanial Anterior, GC, Japan; Charisma Opal, Kulzer, Germany; Beautifil II, Shofu, USA). Samples were immersed in 200 mL water to one effervescent multivitamin tablet (Redoxon Triple Action, Bayer) at 24 °C for 2 min a day in 24 h intervals for 30 days. All samples' surface roughness (Ra) and ΔE(L*a*b) measurements were recorded at the beginning and end of the 30 days. The Wald chi-square and a two-way ANOVA were used for statistical analysis (significance level p < 0.05). The resin composite type and exposure to the multivitamin had a statistically significant effect on Ra values (p < 0.05). The resin composite type had a statistically significant effect on ΔE values, likely due to the higher mean value of BII (p = 0.040). The surface roughness and color of resin composites can be affected by multivitamins with a pH value of 3.0. Therefore, it is important to consider the patient's routine vitamin intake during resin composite selection. Additional research is required to explore the properties of different dental restorative materials.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。