Preparation and Piezocatalytic Performance of γ-AlON Particles for Dye-Pollutant Degradation Under Ultrasonic Vibration

超声振动下γ-AlON粒子的制备及其对染料污染物降解的压电催化性能

阅读:1

Abstract

Piezocatalytic materials have attracted widespread attention in the fields of clean energy and water treatment because of their ability to convert mechanical energy directly into chemical energy. In this study, γ-AlON particles synthesised using carbothermal reduction and nitridation (CRN) were used for the first time as a novel piezocatalytic material to degrade dye solutions under ultrasonic vibration. The γ-AlON particles exhibited good performance as a piezocatalytic material for the degradation of organic pollutants. After 120 min under ultrasonic vibration, 40 mg portions of γ-AlON particles in 50 mL dye solutions (10 mg/L) achieved 78.06%, 67.74%, 74.29% and 64.62% decomposition rates for rhodamine B (RhB), methyl orange (MO), methylene blue (MB) and crystal violet (CV) solutions, respectively; the fitted k values were 13.35 × 10(-3), 10.79 × 10(-3), 12.09 × 10(-3) and 8.00 × 10(-3) min(-1), respectively. The piezocatalytic mechanism of γ-AlON particles in the selective degradation of MO was further analysed in free-radical scavenging activity experiments. Hydroxyl radicals (•OH), superoxide radicals (•O(2)(-)), holes (h(+)) and electrons (e(-)) were found to be the main active substances in the degradation process. Therefore, γ-AlON particles are an efficient and promising piezocatalytic material for the treatment of dye pollutants.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。