Characterisation of Wood Particles Used in the Particleboard Production as a Function of Their Moisture Content

刨花板生产中所用木质颗粒的特性及其含水率

阅读:1

Abstract

The properties of particleboards and the course of their manufacturing process depend on the characteristics of wood particles, their degree of fineness, geometry, and moisture content. This research work aims to investigate the physical properties of wood particles used in the particleboard production in dependence on their moisture content. Two types of particles currently used in the production of three-layer particleboards, i.e., microparticles (MP) for the outer layers of particleboards and particles for the core layers (PCL), were used in the study. The particles with a moisture content of 0.55%, 3.5%, 7%, 10%, 15%, and 20% were tested for their poured bulk density (ρp), tapped bulk density (ρt), compression ratio (k), angle of repose (αR), and slippery angle of repose (αs). It was found that irrespective of the fineness of the particles, an increase in their moisture content caused an increase in the angle of repose and slippery angle of repose and an increase in poured and tapped bulk density, while for PCL, the biggest changes in bulk density occurred in the range up to 15% of moisture content, and for MP in the range above 7% of moisture content, respectively. An increase in the moisture content of PCL in the range studied results in a significant increase in the compression ratio from 47.1% to 66.7%. The compression ratio of MP increases only up to 15% of their moisture content-a change of value from 47.1% to 58.7%.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。