Surface Finish and Back-Wall Dross Behavior during the Fiber Laser Cutting of AZ31 Magnesium Alloy

AZ31镁合金光纤激光切割过程中的表面光洁度和背壁熔渣行为

阅读:1

Abstract

Magnesium alloys are of increasing interest in the medical industry due to their biodegradability properties and better mechanical properties as compared to biodegradable polymers. Fiber laser cutting of AZ31 magnesium alloy tubes was carried out to study the effect of cutting conditions on wall surface roughness and back-wall dross. During the experiments, an argon gas chamber was adapted in order to avoid material reactivity with oxygen and thus better control the part quality. A surface response methodology was applied to identify the significance of pulse overlapping and pulse energy. Our results indicate minimum values of surface roughness (R(a) < 0.7 μm) when the spot overlapping is higher than 50%. A back-wall dross range of 0.24% to 0.94% was established. In addition, a reduction in back-wall dross accumulations was obtained after blowing away the dross particles from inside the tube using an argon gas jet, reaching values of 0.21%. Laser cutting experimental models show a quadratic model for back-wall dross related with the interaction of the pulse energy, and a linear model dependent on pulse overlapping factor for surface roughness.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。