Effects of Thermocycling with Two Different Curing Techniques on Enamel Micro-Cracks Formation, Debonding, and Failure Modes of Ceramic Brackets: An In Vitro Study

两种不同固化技术的热循环对陶瓷托槽牙釉质微裂纹形成、脱粘和失效模式的影响:一项体外研究

阅读:1

Abstract

Despite the rise in popularity of ceramic braces for adults, the risk of enamel microcracks (EMCs) upon removal remains a significant drawback for both dental professionals and patients. Our study aimed to assess the effects of thermocycling, pre-curing, and co-curing techniques with different bonding agents on the enamel surface of teeth after the removal of ceramic brackets. We also examined the incidence, quantity, length, and direction of EMCs on tooth surfaces. Additionally, the adhesive remnant index (ARI) scores and orthodontic bracket bond failure modes were evaluated and compared. The study divided 40 extracted upper canine teeth into ten groups for further analysis. Two groups had intact enamel as the negative control, while the remaining groups had orthodontic ceramic brackets bonded using different bonding agents and curing techniques. Thermocycling was performed in five groups, and ARI was assessed after debonding. The study findings were statistically significant (p < 0.05) in demonstrating the impact of curing techniques on EMCs and debonding outcomes. Seventh-generation bonding agents resulted in complete adhesive removal (ARI = 0). The microcracks' incidence, number, and length showed insignificant results. Differences in ARI between thermocycler and non-thermocycler samples were insignificant. Both co-curing and pre-curing techniques yielded comparable ARI results. This study highlights the importance of using advanced bonding agents to minimize enamel damage during ceramic bracket debonding.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。