An In vitro Shear Bond Strength Study to Evaluate the Efficacy of Moisture-Insensitive Primer

体外剪切粘结强度研究,以评估对水分不敏感的底涂剂的功效

阅读:1

Abstract

AIMS: We aimed to evaluate and compare the efficacy of moisture-insensitive primer (MIP) Transbond MIP while bonding to wet enamel surface. MATERIALS AND METHODS: This study was done on 100 freshly extracted human premolar teeth, collected from the Department of Oral Surgery, Government Dental College, Calicut. They were stored in distilled water at room temperature. All teeth were healthy and without caries lesion, no evidence of surface defects, or any developmental morphological aberrations. Teeth were divided into 5 groups of twenty each for the testing and Brackets were bonded onto the tooth surface in 5 different bonding sequences using Transbond XT and Transbond MIP.. RESULTS: All the three groups of MIP have gained statistically significant higher SBS compared to Group I (Transbond XT primer in wet). Marked decrease in SBS of Transbond XT resin in wet environment was deduced. MIP in repriming sequence (Group IV) is found to have higher bond strength than other MIP groups. CONCLUSIONS: Clinical acceptability of Transbond MIP in wet environment could be recommended. MIP repriming should be done in cases where there is a doubt of contamination with saliva after initial primer application.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。