Effect of storage environment on the bond strength of reattachment of crown fragments to fractured teeth

储存环境对牙冠碎片与断裂牙齿再粘接强度的影响

阅读:1

Abstract

AIM: The aim of this study was to examine various storage environments for storing fragments before being bonded to the remaining teeth and also estimate the required force to fracture the restored teeth. MATERIALS AND METHODS: Sixty mandibular incisor teeth were fractured on the incisal one-third and were divided into five groups of 12 each to be stored in normal saline, water, milk, saliva and dry environments for 24 hours. All the fractured parts in each group were bonded to their relevant apical parts by an etch and rinse bonding system and a flowable composite resin. The fracture resistance was measured by a universal testing machine, and the results were analyzed using one-way ANOVA and Tukey statistical tests. RESULTS: The results revealed that the difference among the five groups was statistically significant (P<0.001). Tukey tests showed that the force required for fracturing fragments kept in the milk and saliva environments were significantly higher than those for the normal saline, water and dry environments (P<0.05 ). CONCLUSIONS: It was concluded that keeping the fractured parts in milk and saliva environments can increase the required force for fracturing teeth more than the other environments.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。