Shear Bond Performance at Interface of Concrete-Filled Steel Tube after Freeze-Thaw Cycles

混凝土填充钢管界面在冻融循环后的剪切粘结性能

阅读:2

Abstract

The shear bond performance between steel tube and concrete is the basis of a synergistic effect between two materials. When a concrete-filled steel tube structure is damaged by freeze and thaw cycles, the shear bond performance will deteriorate, which will inevitably affect the safety of the structure. In this paper, the effects of the numbers of freeze-thaw cycles, section type of steel tube, and concrete strength on the failure mode, bond strength, and peak slip of concrete-filled steel tube are investigated. In addition, the load-slip curve, the shear bond strength calculation formula, and the peak slip calculation formula are obtained. The results show that the shear bond performance decreases with the increase in freeze and thaw cycles; after 20 freeze and thaw cycles, the shear bond strength of the round steel tube specimen with 30 MPa decreases by 33.33%, while that of peak slip increases by 11.49%; the shear bond strength increases with the increase in concrete strength, while the degree of decrease in shear bond strength after freeze-thaw cycles is reduced; the shear bond strength of the round steel tube push-out specimen is higher than that of square steel tube push-out specimen, and after 20 freeze and thaw cycles, the shear bond strength of the round steel tube push-out specimen with 30 MPa/45 MPa is 0.86 MPa/1.62 MPa, while that of square steel tube push-out specimen with 30 MPa/45 MPa is 0.40 MPa/0.50 MPa.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。