Application of drag-reducing polymer solutions as test fluids for in vitro evaluation of potential blood damage in blood pumps

应用减阻聚合物溶液作为测试流体体外评估血泵的潜在血液损伤

阅读:8
作者:Amanda R Daly, Hideo Sobajima, Salim E Olia, Setsuo Takatani, Marina V Kameneva

Abstract

In vitro evaluation of the potential of a circulatory-assist device to damage blood cells has generally been performed using blood from various species. Problems with this approach include the variability of blood sensitivity to mechanical stress in different species, preparation of blood including the adjustment of hematocrit to a standard value, changes in the mechanical properties of blood that occur during storage, and necessity to pool blood samples to obtain an adequate amount of blood for in vitro circulating systems. We investigated whether the mechanical degradation of a drag-reducing polymer (DRP) solution resulting in the loss of drag-reducing ability can indicate the degree of shear-induced blood damage within blood pumps. DRP solution (polyethylene oxide, 4,500 kDa, 1,000 ppm) or porcine blood were driven through a turbulent flow system by a centrifugal pump, either the Bio-Pump BPX-80 (Medtronic, Inc.) or CentriMag (Levitronix LLC) at a constant pressure gradient of 300 mm Hg for 120 minutes. DRP mechanical degradation was evaluated by reduction of flow rate and solution viscosity. A proposed index of DRP mechanical degradation (PDI) is similar to the normalized index of hemolysis (NIH) typically used to quantify the results of in vitro testing of blood pumps. Results indicate that the mechanical degradation of DRP solutions may provide a sensitive standard method for the evaluation of potential blood trauma produced by blood pumps without the use of blood.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。