Improving the quality of soluble dietary fiber from Poria cocos peel residue following steam explosion

利用蒸汽爆破法提高茯苓皮残渣中可溶性膳食纤维的质量

阅读:3

Abstract

Poria cocos peel residue (PCPR) still contains much soluble dietary fiber (SDF), steam explosion (SE) treatment was applied to PCPR to create a superior SDF. Steam pressure of 1.2 MPa, residence period of 120 s, and moisture content of 13% were the optimized parameters for SE treatment of PCPR. Under optimized circumstances, SE treatment of PCPR enhanced its SDF yield from 5.24% to 23.86%. Compared to the original SDF, the SE-treated SDF displayed improved enzyme inhibition, including the inhibition of α-amylase and pancreatic lipase, also enhanced water holding, oil holding, water swelling, nutrient adsorption including cholesterol, nitrite ions, and glucose and antioxidant abilities. Additionally, it had a decreased molecular weight, improved thermal stability, and a rough surface with many pores of different sizes. Given that SDF had been improved physiochemical and functional characteristics thanks to SE treatment, it might be the excellent functional ingredient for the food business.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。