Fracture Resistance of CAD/CAM Implant-Supported 3Y-TZP-Zirconia Cantilevers: An In Vitro Study

CAD/CAM种植体支持的3Y-TZP-氧化锆悬臂梁的抗断裂性能:一项体外研究

阅读:2

Abstract

(1) Introduction: Implant-supported fixed complete dentures are mostly composed of cantilevers. The purpose of this work was to evaluate the fracture resistance of zirconia (Prettau®, second generation, or Ice Zirkon Translucent, first generation) with cantilever lengths of 6 and 10 mm, and zirconia’s fracture resistance in relation to an average bite force of 250 N. (2) Materials and methods: Forty structures were created in CAD/CAM and divided into four groups: group A (6 mm cantilever in IZT), group B (10 mm cantilever in IZT), group C (6 mm cantilever in Pz), and group D (10 mm cantilever in pz). The study consisted of a traditional “load-to-failure” test. (3) Results: A statistically significant result was found for the effect of cantilever length, t(38) = 16.23 (p < 0.001), with this having a large effect size, d = 4.68. The 6 mm cantilever length (M = 442.30, sd = 47.49) was associated with a higher mean force at break than the 10 mm length (M = 215.18, sd = 40.74). No significant effect was found for the type of zirconia: t(38) = 0.31 (p = 0.757), and d = 0.10. (4) Conclusions: All the components with cantilever lengths of 6 mm broke under forces higher than 250 N. Cantilevers larger than 10 mm should be avoided.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。