Distorting crack-front geometry for enhanced toughness by manipulating bioinspired heterogeneity

通过操控仿生异质性来改变裂纹前沿几何形状,从而提高韧性

阅读:1

Abstract

Control of crack propagation is crucial to make tougher heterogeneous materials. As a crack interacts with material heterogeneities, its front distorts and adopts complex tortuous configurations. While the behavior of smooth cracks with straight fronts in homogeneous materials is well understood, the toughening by rough cracks with tortuous fronts in heterogeneous materials remains unsolved. Here we highlight a distorted crack-front geometric toughening mechanism by manipulating bioinspired anisotropic heterogeneities of microstructural orientations and component properties. We reveal theoretically and demonstrate experimentally that the local mixed-mode I + II + III fracture triggered by local anisotropic heterogeneities lead to a helical crack front in a representative heterogeneous system with bioinspired twisted plywood structures under remote mode I loading. An anomalous nonlinear law of both the enhanced fracture resistance and the helical crack-front length versus the microstructural orientation is revealed, in contrast to the linear toughening law ignoring the hidden 3D topography within crack fronts. An optimization design protocol towards toughness amplification is developed by parametrically manipulating anisotropic heterogeneities to helically distort crack front. Our findings not only provide physical insights into the origin of biological heterogeneities modulated tortuous crack fronts but also offer a benchmark solution for enhancing toughness by parametrically engineering spatial heterogeneities.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。